Physical Properties Metric English Comments
Viscosity 1.68e+6 cP

@Temperature 130 °C
1.68e+6 cP

@Temperature 266 °F
Melt; ISO 1133
Lubrizol Advanced Materials Pearlbond® ECO D590 Thermoplastic Polyurethane
Pearlbondâ„¢ ECO D590 is a linear, aromatic bio-polyurethane based on specialty polyol from renewable sources, supplied in form of white spherical granules, with an extremely high crystallization..