Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 1.68e+6 cP @Temperature 130 °C |
1.68e+6 cP @Temperature 266 °F |
Melt; ISO 1133 |
Lubrizol Advanced Materials Pearlbond® ECO D590 Thermoplastic Polyurethane Pearlbond™ ECO D590 is a linear, aromatic bio-polyurethane based on specialty polyol from renewable sources, supplied in form of white spherical granules, with an extremely high crystallization.. |