Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 120000 - 175000 cP | 120000 - 175000 cP | |
ND Industries 907 Anti-seize Aluminum-Graphite Aluminum and Graphite based, general purpose lubricant |
|||
Viscosity | 120000 - 175000 cP | 120000 - 175000 cP | |
ND Industries 907 Anti-seize Copper-Graphite Copper and graphite based lubricant for softer metals |
|||
Viscosity | 120000 cP | 120000 cP | Melt Viscosity, 260°C, 1500 sec-1; ISO 11443 |
SABIC Innovative Plastics GELOY XTPM405 ASA+PC High flow PC/ASA with improved impact at room and low temperatures. Improved release. Excellent weatherability for outdoor unpainted or clearcoated applications. Injection Moldable with large color .. |
|||
Viscosity | 120000 - 480000 cP @Temperature 260 - 260 °C |
120000 - 480000 cP @Temperature 500 - 500 °F |
Average value: 204000 cP Grade Count:22 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Viscosity | 120000 - 480000 cP @Shear Rate 1000 - 1000 1/s |
120000 - 480000 cP @Shear Rate 1000 - 1000 1/s |
Average value: 204000 cP Grade Count:22 |
Overview of materials for Polycarbonate/ABS Alloy, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/ABS Alloy, Unreinforced". Each property range of values reported is minimum and maximum va.. |
|||
Viscosity | 120000 cP | 120000 cP | Mixed Viscosity (Thixotropic gel) |
ITW Devcon Composite Welderâ„¢ Methacrylate Adhesive FS, Blue Green, Black Information provided by ITW Devcon |
|||
Viscosity | 120000 - 135000 cP @Temperature 23.0 °C |
120000 - 135000 cP @Temperature 73.4 °F |
|
Master Bond Supreme 3HT High Bond Strength One Component Epoxy Adhesive System Master Bond Polymer System Supreme3HT is a storage stable one component, heat curing epoxy adhesive featuring a hither to unattainable balance of performance properties including both high shear and.. |
|||
Viscosity | 120000 cP @Temperature 25.0 °C |
120000 cP @Temperature 77.0 °F |
Mixed (sp #4, 0.3 rpm) |
Tra-Con Tra-Bond FS443 Color Keyed Thixotropic Epoxy Adhesive TRA-BOND FS443 is a fast cure, high viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating s.. |
|||
Viscosity | 120000 - 140000 cP @Temperature 23.0 °C |
120000 - 140000 cP @Temperature 73.4 °F |
|
Master Bond EP21TDC-7 Highly Flexible Two Component Epoxy System Master Bond Polymer System EP21TDC-7 is a two component highly flexible epoxy resin system for high performance bonding, sealing, and coating. It is formulated to cure at ambient temperatures or mor.. |
|||
Viscosity | 120000 cP @Shear Rate 1000 1/s, Temperature 260 °C |
120000 cP @Shear Rate 1000 1/s, Temperature 500 °F |
melt viscosity; b.o. ISO 11443-A |
Covestro Bayblend® FR3005 HG PC/ABS Blend Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Flame-retardant• Injec.. |
|||
Viscosity | 120000 cP @Temperature 190 °C |
120000 cP @Temperature 374 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 120000 cP @Temperature 190 °C |
120000 cP @Temperature 374 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1309E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 120000 cP @Temperature 160 °C |
120000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1516A Heat Stabilized Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 120000 cP @Temperature 160 °C |
120000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1666A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 120000 cP | 120000 cP | with shear thinning |
3M FireDam™ 200 Spray 3M Fire Dam Spray 200 is a sprayable water-based material that dries to form a tough, elastomeric coating. This material is used to firestop perimeter joints (curtain wall), construction joints and .. |
|||
Viscosity | 120000 cP | 120000 cP | Part A |
3M Scotchkote™ 323 Purple Patch Compound 3M Scotchkote 323 Purple Patch Compound is an ambient temperature cure, two-part system designed to protect metal, concrete and other surfaces from corrosion and deterioration. Scotchkote 323 Purple.. |
|||
Viscosity | 120000 cP @Temperature 23.0 °C |
120000 cP @Temperature 73.4 °F |
|
Master Bond UV15X-5 One Component High Viscosity UV Curable System Master Bond Polymer System UV15X-5 is one component, non-yellowing, UV curable urethane elastomer system possessing high flexibility and outstanding abrasion resistance. This high viscosity system c.. |