Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 70000 - 140000 cP | 70000 - 140000 cP | Part B |
Master Bond EP21TDCHT-LO Room Temperature Curing, Toughened Two Component Epoxy Master Bond Polymer Adhesive EP21TDCHT-LO is a two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a very forgiving and convenient one .. |
|||
Viscosity | 80000 - 140000 cP | 80000 - 140000 cP | at 20 RPM; Thixotropic |
Loctite® 334 Acrylic Bonding Adhesive Acrylic Bonding AdhesivesLoctite® Acrylic Adhesives were developed for bonding applications that require tensile, shear and peel strength combined with maximum impact, stress and shock resistance. .. |
|||
Viscosity | 120000 - 140000 cP @Temperature 23.0 °C |
120000 - 140000 cP @Temperature 73.4 °F |
|
Master Bond EP21TDC-7 Highly Flexible Two Component Epoxy System Master Bond Polymer System EP21TDC-7 is a two component highly flexible epoxy resin system for high performance bonding, sealing, and coating. It is formulated to cure at ambient temperatures or mor.. |
|||
Viscosity | 100000 - 140000 cP @Temperature 23.0 °C |
100000 - 140000 cP @Temperature 73.4 °F |
2.5 rpm |
Epoxy Technology EPO-TEK® OG159-2 UV Cure Optical Epoxy Material Description: A single component, high viscosity, UV curable epoxy adhesive designed for sealing glass plates together in the LCD/OLED/display industry. It contains 1mil glass beads for bon.. |