Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 262300 cP @Shear Rate 500 1/s, Temperature 305 °C |
262300 cP @Shear Rate 500 1/s, Temperature 581 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66
(Unverified Data**) 20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf.. |