Polymer Property : Viscosity = 262300 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 262300 cP

@Shear Rate 500 1/s,
Temperature 305 °C
262300 cP

@Shear Rate 500 1/s,
Temperature 581 °F
ISO 11403-1 -2
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66  (Unverified Data**)
20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf..