Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 900000 - 3.00e+6 cP @Temperature 190 - 190 °C |
900000 - 3.00e+6 cP @Temperature 374 - 374 °F |
Average value: 1.60e+6 cP Grade Count:15 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |
|||
Viscosity | 900000 - 3.00e+6 cP @Shear Rate 50.0 - 50.0 1/s |
900000 - 3.00e+6 cP @Shear Rate 50.0 - 50.0 1/s |
Average value: 1.60e+6 cP Grade Count:15 |
Overview of materials for Anhydride-Modified Polyethylene This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o.. |