Physical Properties Metric English Comments
Viscosity 900000 - 3.00e+6 cP

@Temperature 190 - 190 °C
900000 - 3.00e+6 cP

@Temperature 374 - 374 °F
Average value: 1.60e+6 cP Grade Count:15
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..
Viscosity 900000 - 3.00e+6 cP

@Shear Rate 50.0 - 50.0 1/s
900000 - 3.00e+6 cP

@Shear Rate 50.0 - 50.0 1/s
Average value: 1.60e+6 cP Grade Count:15
Overview of materials for Anhydride-Modified Polyethylene
This property data is a summary of similar materials in the MatWeb database for the category "Anhydride-Modified Polyethylene". Each property range of values reported is minimum and maximum values o..
Viscosity >= 900000 cP
>= 900000 cP
Part B, thixotropic
Master Bond EP76M-F Electrically Conductive, Two Part Epoxy
Description: Master Bond EP76M-F is a two component, nickel filled, electrically conductive epoxy system for high performance bonding, sealing, and coating formulated to cure at room temperature or ..
Viscosity 900000 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
900000 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Bynel® 4288 Anhydride-Modified LDPE Adhesive Resin
Bynel® Series 4200 resins are anhydride-modified, low-density polyethylene resins. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process ..
Viscosity 900000 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
900000 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Bynel® 1123 Modified EVA Adhesive Resin
Bynel® Series 1100 resins are modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process polyethylen..
Viscosity 900000 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
900000 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Bynel® 3810 Anhydride-Modified Ethylene Vinyl Acetate Adhesive Resin
Bynel® Series 3800 resins are anhydride-modified ethylene vinyl acetate polymers. They are available in pellet form for use in conventional extrusion and coextrusion equipment designed to process p..
Viscosity 900000 cP

@Shear Rate 50.0 1/s,
Temperature 190 °C
900000 cP

@Shear Rate 50.0 1/s,
Temperature 374 °F
estimated from log-log graph
DuPont Bynel® 2174 Anhydride-Modified Ethylene Acrylate Adhesive Resin  (discontinued **)
Bynel® Series 2100 resins are anhydride-modified ethylene acrylate resins. They contain a temperature stable ester that makes them functional in high temperature coextrusions. They are available in..