Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 30198 cP @Temperature 25.0 °C |
30198 cP @Temperature 77.0 °F |
Mixed (cp #52, 10 rpm) |
Tra-Con Tra-Duct 926K01 Long Work Life Flexible Silver-Filled Epoxy Adhesive TRA-DUCT 926K01 is recommended for electronic bonding, coating and sealing applications that require high flexibility coupled with excellent electrical and mechanical properties. This two-part epoxy.. |