Polymer Property : Viscosity = 30198 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 30198 cP

@Temperature 25.0 °C
30198 cP

@Temperature 77.0 °F
Mixed (cp #52, 10 rpm)
Tra-Con Tra-Duct 926K01 Long Work Life Flexible Silver-Filled Epoxy Adhesive
TRA-DUCT 926K01 is recommended for electronic bonding, coating and sealing applications that require high flexibility coupled with excellent electrical and mechanical properties. This two-part epoxy..