Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 45000 cP @Pressure 0.621 MPa |
45000 cP @Pressure 90.0 psi |
Servers; ASTM D-1823 |
SABIC PVC 741E Emulsion Polyvinyl Chloride for Paste Preparation Product Description: PVC 741E is a fine particle, high molecular weight PVC homopolymer, made by emulsion polymerization. It is designed for the manufacture of plastisols exhibiting low viscositie.. |
|||
Viscosity | 45000 cP @Temperature 175 °C |
45000 cP @Temperature 347 °F |
Automatic orifice Viscosity |
Cookson Group Plaskon® SMT-B-1 LAS (146.408) Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for grid arrays (BGA/LGA) requiring low alpha particle count. It is formulated .. |
|||
Viscosity | 45000 - 65000 cP @Temperature 40.0 °C |
45000 - 65000 cP @Temperature 104 °F |
|
Taiwan PU Corporation PTMG CPU-42L Polyurethane Casting Elastomer A urethane elastomer that can be cured by reacting with a polyamine or a polyolhardener. The molding process is composed of pre-heating, degassing, maxing with a hardener, pouring into the mold, cu.. |
|||
Viscosity | 45000 cP | 45000 cP | Before Curing |
Silikony Polskie Gumosil M Silicone Rubber Flexible with good tearing resistance |
|||
Viscosity | 45000 cP | 45000 cP | Before Curing |
Silikony Polskie Polastosil M-56 Silicone Rubber Rubber with strong hardness |
|||
Viscosity | 45000 cP | 45000 cP | |
Master Bond Mastersil 800 One Component, Room Temperature Curing Silicone MasterSil 800 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed-in-place gaskets. This specialty system features ultra high temp.. |
|||
Viscosity | 45000 cP | 45000 cP | Haake cone and plate rheometer @ 5/sec (35mm/2° cone) |
Loctite® 3565 High performance epoxy, high Tg and low CTE High Tg Underfill COB/DCA Encapsulants are essential to the reliability of flip chip assemblies because they minimize the thermal mismatch between the flip chip and substrate.Loctite® Underfills and Encapsulants imp.. |
|||
Viscosity | 45000 - 75000 cP | 45000 - 75000 cP | Part A |
Master Bond EP30LTE-LO Dimensionally Stable Low Outgassing Two Part Epoxy Master Bond Polymer System EP30LTE-LO is a thermal shock resistant epoxy resin system with low thermal expansion properties and dimensional stability for high performance bonding, sealing and castin.. |
|||
Viscosity | 45000 cP | 45000 cP | Resin (cp #52, 10 rpm) |
Tra-Con Tra-Bond 216R01 Fire Retardant Epoxy TRA-BOND 216R01 is a fast curing material with a set time of 5 to 7 minutes. Samples tested were certified to the requirements of UL94 V-O, and is RoHS compliant. TRA-BOND 216R01 develops significa.. |
|||
Viscosity | 45000 cP | 45000 cP | dynamic |
Dow Corning 736 HEAT RESISTANT/SEALANT Red RTV adhesive/sealant for temperatures up to 600F/315CInformation provided by Dow Corning |
|||
Viscosity | 45000 cP @Temperature 25.0 °C |
45000 cP @Temperature 77.0 °F |
|
Cytec (Conap) RN-1210 / EA-87 Conapoxy® Resin / Conacure® Hardener Epoxy Potting and Encapsulating Systems for Electronic ApplicationsHigh technology epoxy resin systems for potting and encapsulation, for the defense, aerospace, electronics, computer, automotive an.. |
|||
Viscosity | 45000 - 70000 cP @Temperature 23.0 °C |
45000 - 70000 cP @Temperature 73.4 °F |
50 rpm |
Epoxy Technology EPO-TEK® OE100-T High Temperature Epoxy Material Description: A two component, high Tg, high temperature grade epoxy designed for semiconductor, underfill, hard-disk drive and hybrid micro-electronics packaging applications. The epoxy ca.. |
|||
Viscosity | 45000 cP | 45000 cP | |
Epoxyset Epoxibond EB-347 Low Expansion Epoxy Adhesive EB-347 is a highly filled, low coefficient expansion, epoxy adhesive. This low out-gassing adhesive exhibits excellent wettability without preheating metal bonding surfaces and has a good dimensiona.. |
|||
Viscosity | 45000 cP | 45000 cP | dynamic |
Dow Corning 3-3442 FLOWABLE TEXTILE SEALANT A flowable one part acid curing rtv silicone for elastomeric coatings.Information provided by Dow Corning |
|||
Viscosity | 45000 cP | 45000 cP | |
Dymax 9003v3.0 Flexible Clear Microencapsulant High Performance Light-Curing Adhesives and Coatings for Electronic AssemblyDymax 9003v3.0 Flexible Clear MicroencapsulantGlob top for photosensing devices Cure Type: UV/Visible Typical Use: Optic.. |
|||
Viscosity | 45000 cP | 45000 cP | |
ACC MM850 Low Tear Condensation Cure 2-Part Molding Rubber Part of the Amber Chemical Group. Data provided by manufacturer.Characteristics: low viscosity, good resistance to styrene attack, easy degassing, low shrinkage, range of catalysts. Applications: sh.. |
|||
Viscosity | 45000 cP | 45000 cP | Base |
ACC QM 135 QSI Quantum Silicones 35 Durometer Condensation Cured Moldmaking Material QM 135 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent cho.. |
|||
Viscosity | 45000 cP | 45000 cP | B Component; ASTM D1824 |
Aptek 2201-A/B Fast set urethane adhesive APTEK 2201-A/B is a two component, dark gray, urethane adhesive system displaying excellent adhesion to various plastic, wood, ceramic, and metal substrates. APTEK 2201-A/B is capable of achieving f.. |
|||
Viscosity | 45000 cP | 45000 cP | Mixed Viscosity |
Aremco Aremco-Bond™ 2310 High Performance Epoxide Ceramic-Filled, 1:1, High Lap Shear and Peel Strength, Autoclavable. |
|||
Viscosity | 45000 - 85000 cP | 45000 - 85000 cP | |
3M Pronto™ CA-50 Gel Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A high-viscosity gel consistenc.. |
|||
Viscosity | 45000 cP | 45000 cP | Base |
ACC QM 262 QSI Quantum Silicones 60 Durometer Addition Cure Moldmaking Material QM262 is a two component, room temperature, addition cure silicone material. The cured rubber has excellent mechanical properties, good shelf-life stability, excellent physical properties and resin .. |
|||
Viscosity | 45000 cP @Temperature 25.0 °C |
45000 cP @Temperature 77.0 °F |
Mixed |
Trelleborg Emerson & Cuming Stycast® 4640-25 Two-Component Silicone Flexible Encapsulant Emerson & Cuming 4640-25 Stycast® Two-Component Silicone Flexible EncapsulantDescriptionAn RTV condensation cure. Pourable and room temperature curable.FeaturesHigh TemperaturePoor Chemical Resista.. |
|||
Viscosity | 45000 cP | 45000 cP | Mixed; TM R050-12 |
Resinlab® EP1200 Black Casting Resin Resinlab™ EP1200 Black is a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility and a low CTE. It meets the re.. |
|||
Viscosity | 45000 cP | 45000 cP | Part A, RVT, #7, 20 rpm; TM R050-12 |
Resinlab® EP1305LV Black Epoxy Casting Resin Resinlab™ EP1305LV Black is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |
|||
Viscosity | 45000 cP | 45000 cP | Part A, RVT, #7, 20 rpm; TM R050-12 |
Resinlab® EP1305LV Clear Epoxy Casting Resin Resinlab™ EP1305LV Clear is a black two-part epoxy casting resin designed to give good adhesion to metals and especially PVC. It has good wetting to most surfaces and is free flowing to penetrate c.. |