Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 24000 - 46000 cP @Temperature 23.0 °C |
24000 - 46000 cP @Temperature 73.4 °F |
5 rpm |
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy Material Description: Silver-filled, electrically conductive, flexible epoxyInformation Provided by Epoxy Technology |