Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 200000 - 5.00e+6 cP @Temperature 240 - 280 °C |
200000 - 5.00e+6 cP @Temperature 464 - 536 °F |
Average value: 1.26e+6 cP Grade Count:6 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
Viscosity | 200000 - 5.00e+6 cP @Shear Rate 0.100 - 1000 1/s |
200000 - 5.00e+6 cP @Shear Rate 0.100 - 1000 1/s |
Average value: 1.26e+6 cP Grade Count:6 |
Overview of materials for Nylon 6, Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat.. |