Polymer Property : Viscosity = 510000 cP Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Viscosity 510000 - 650000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
510000 - 650000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-810 Polyetheretherketone (PEEK)
KetaSpire® KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0.50 kPa-s for standard high-viscosity PEEK grades ..
Viscosity 510000 - 650000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
510000 - 650000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Solvay Specialty Polymers KetaSpire® KT-810FP Polyetheretherketone (PEEK)
KetaSpire® KT-810FP is the fine powder form of KT-810 resin. KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0..
Viscosity 510000 cP
510000 cP
A
Shin-Etsu Silicones LIMSâ„¢ KE2095-50AB Elastomer
KE-2095-50 is a selective self-adhesive liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is lo..
Viscosity 510000 cP

@Shear Rate 300 1/s,
Temperature 190 °C
510000 cP

@Shear Rate 300 1/s,
Temperature 374 °F
ASTM D3835
Advanced Polymer Alloys Alcryn® 4670 BK Melt Processable Rubber
Alcryn melt-processable rubber (MPR) is a true rubber, based on a partially cross-linked, chlorinated olefin interpolymer alloy. Alcryn is designed for the manufacture of rubber parts with high prod..