Solvay Specialty Polymers KetaSpire® KT-810FP Polyetheretherketone (PEEK)

Category Polymer , Thermoplastic , Polyketone , Polyetheretherketone (PEEK)
Manufacturer Solvay Specialty Polymers
Trade Name KetaSpire®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers KetaSpire® KT-810FP Polyetheretherketone (PEEK).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
KetaSpire® KT-810FP is the fine powder form of KT-810 resin. KT-810 is an ultra-high molecular weight natural PEEK resin having a melt viscosity ranging from 0.51-0.65 kPa-s as compared to 0.38-0.50 kPa-s for standard high-viscosity PEEK grades such as KT-820 and its fine powder analog KT-820FP. KetaSpire® PEEK is produced to the highest industry standards and is characterized by a distinct combination of properties, which include excellent chemical resistance to organics, acids and bases; exceptional retention of mechanical properties up to 300°C (572°F); best-in-class fatigue resistance; excellent wear resistance; ease of melt processing; and high purity. The KT-810 grade achieves a greater level of mechanical toughness than previously possible with PEEK, yet it is still processable by conventional methods including extrusion, injection molding, and compression molding.Features: Autoclave Sterilizable; Ductile; E-beam Sterilizable; Ethylene Oxide Sterilizable; Fatigue Resistant; Flame Retardant; Good Chemical Resistance; Good Dimensional Stability; Good Impact Resistance; Good Sterilizability; Heat Sterilizable; High Heat Resistance; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam SterilizableUses: Aircraft Applications; Automotive Applications; Connectors; Dental Applications; Electrical/Electronic Applications; Film; Gears; Hospital Goods; Housings; Industrial Applications; Medical Devices; Medical/Healthcare Applications; Oil/Gas Applications; Pump Parts; Seals; Surgical Instruments; TubingAdditional Properties: Particle Size - 0.00 %; Particle Size - < 2.00 %Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.29 g/cc
0.0466 lb/in³
ASTM D792
Water Absorption 0.10 %

@Time 86400 sec
0.10 %

@Time 24.0 hour
ISO 62
Viscosity 510000 - 650000 cP

@Shear Rate 1000 1/s,
Temperature 400 °C
510000 - 650000 cP

@Shear Rate 1000 1/s,
Temperature 752 °F
Melt Viscosity; ASTM D3835
Mechanical Properties Metric English Comments
Tensile Strength, Yield 94.5 MPa
13700 psi
ASTM D638
Elongation at Break 25 - 50 %
25 - 50 %
ASTM D638
Elongation at Yield 5.2 %
5.2 %
ASTM D638
Tensile Modulus 3.50 GPa
508 ksi
ASTM D638
Flexural Strength 145 MPa
21000 psi
ASTM D790
Flexural Modulus 3.70 GPa
537 ksi
ASTM D790
Izod Impact, Notched 1.00 J/cm
1.87 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 157 °C

@Thickness 3.20 mm
315 °F

@Thickness 0.126 in
Annealed; ASTM D648
Descriptive Properties Value Comments
Additive Lubricant
Agency Ratings ISO 10993; ISO 10993-Part 1
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Natural
Form Powder
Processing Technique Compression Molding; Extrusion Blow Molding
Film Extrusion; Injection Molding; Machining
Profile Extrusion; Thermoforming; Wire & Cable Extrusion
RoHS Compliance RoHS Compliant
Users viewing this material also viewed the following: