Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 650000 - 650000 cP @Temperature 420 - 420 °C |
650000 - 650000 cP @Temperature 788 - 788 °F |
Average value: 650000 cP Grade Count:1 |
Overview of materials for Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetherketoneetherketoneketone (PEKEKK), Carbon Fiber Filled". Each property range of values reported .. |
|||
Viscosity | 650000 cP @Temperature 420 °C |
650000 cP @Temperature 788 °F |
melt; ISO 11443 |
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, .. |
|||
Viscosity | 650000 cP @Temperature 160 °C |
650000 cP @Temperature 320 °F |
Melt viscosity @ 2.16 kg; ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 120 Linear Thermoplastic Polyurethane Pearlbond® 120 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticity .. |
|||
Viscosity | 650000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
650000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt Viscosity; ASTM D3835 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK), 30% Glass Fiber AvaSpire® AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire® AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This r.. |
|||
Viscosity | 650000 cP | 650000 cP | A |
Shin-Etsu Silicones LIMSâ„¢ KE2004-20A/B Elastomer Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Viscosity | 650000 cP @Shear Rate 0.100 1/s, Temperature 240 °C |
650000 cP @Shear Rate 0.100 1/s, Temperature 464 °F |
|
DSM Akulon® F127 PA6 Low/Medium Viscosity, Film Extrusion |
|||
Viscosity | 650000 cP @Temperature 160 °C |
650000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® 1A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 650000 cP @Temperature 160 °C |
650000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® 1A Copolyamide Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 650000 cP @Temperature 160 °C |
650000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1442E Copolyester Hotmelt Adhesive (Technical Applications) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Viscosity | 650000 cP @Temperature 160 °C |
650000 cP @Temperature 320 °F |
2.16 kg load; ISO 1133 |
EMS-Griltech Griltex® D 1564A Heat Stabilized Copolyamide Hotmelt Adhesive (Technical Applications) GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides for excellent r.. |
|||
Viscosity | 650000 cP @Shear Rate 1000 1/s, Temperature 400 °C |
650000 cP @Shear Rate 1000 1/s, Temperature 752 °F |
Melt; ASTM D3835 |
Solvay Specialty Polymers AvaSpire® AV-621 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 GF30 is a 30% glass fiber reinforced version of AvaSpire AV-621. This formulation offers better dimensional stability and lower warpage than 30% glass reinforced PEEK. This resin ret.. |