Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 9500 - 14000 cP @Shear Rate 230 1/s, Temperature 25.0 °C |
9500 - 14000 cP @Shear Rate 230 1/s, Temperature 77.0 °F |
Haake VT 550 PK1.1° |
Gwent Electronic Materials D2080121D12 Dielectric Ink This product is a thermoplastic screen printing ink, developed for use for flexible polymer applications. It is printed on to flexible polymeric substrates, such as Polyimide and PET substrates, to .. |
|||
Viscosity | 9500 cP @Shear Rate 10994 1/s, Temperature 210 °C |
9500 cP @Shear Rate 10994 1/s, Temperature 410 °F |
ASTM D3835 |
STAR Thermoplastic Alloys & Rubbers StarTUFF TF 45-LR-1 TPE Product Description: StarTUFF TF 45-LR-1 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelHigh Tear strengthHigh Tensile strengthProcessing Method: Injection M.. |
|||
Viscosity | 9500 cP @Temperature 25.0 °C |
9500 cP @Temperature 77.0 °F |
Dynamic |
Struktol POLYDIS 3622 Elastomer modified epoxy prepolymer Applications: STRUKTOL VP 3622 is used where conventional epoxy systems and prepolymers are unable to satisfy the demands of for example impact, flexural and peel strength.Information provided by St.. |
|||
Viscosity | 9500 cP | 9500 cP | 1.9% NaCl added |
Solvay MACKADET® CA-ND Surfactant Product description: Mackadet CA-ND is a concentrated blend of mild surfactants for use as a base for high foaming surfactant systems. Mackadet CA-ND responds rapidly to viscosity building with the .. |
|||
Viscosity | 9500 cP | 9500 cP | 16% Solid, 0.5% NaCl |
Solvay MACKADET® EQ-178 Surfactant Product Description: Mackadet EQ-178 is a mild, concentrated blend of surfactants for use as a base for high foam personal care products. This blend is free of alcohol, diethanolamides, lauryl sulfa.. |
|||
Viscosity | 9500 cP @Temperature 25.0 °C |
9500 cP @Temperature 77.0 °F |
Mixed (cp #52, 10 rpm) |
Tra-Con Tra-Duct 916H01 Electronically Conductive Silver-Filled Epoxy TRA-DUCT 916H01 is an electronically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical .. |
|||
Viscosity | 9500 cP @Temperature 25.0 °C |
9500 cP @Temperature 77.0 °F |
Mixed (cp #52, 10 rpm) |
Tra-Con Tra-Duct 921H01 Information provided by Tra-Con Inc. |
|||
Viscosity | 9500 cP | 9500 cP | |
Loctite® 272 High Temperature/High Strength Threadlocker ThreadlockersInvented by Loctite Corporation as a revolutionary method to lock and seal threaded fasteners, Loctite® Liquid Threadlockers have found wide acceptance in a range of applications--from.. |
|||
Viscosity | 9500 cP | 9500 cP | |
Abatron AboCast 22-30/AboCure 50-12 Epoxy AboCast 22-30 is a black filled resin with high viscosity and a weight of 12.4 lbs/gallon. AboCure 50-12 is clear, fast converter with low viscosity and a weight of 8.2 lbs/gallon. AboCast 22-30/Abo.. |