Polymer Property : Apparent Bulk Density = 0.00903 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.150 - 0.250 g/cc
0.00542 - 0.00903 lb/in³
NanoAmor 95%; OD: 200-500 nm Carbon Nanofibers
ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto..
Apparent Bulk Density 0.150 - 0.250 g/cc
0.00542 - 0.00903 lb/in³
NanoAmor 95%; OD: 200-500 nm Graphitized Carbon Nanofibers
ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas sto..