NanoAmor 95%; OD: 200-500 nm Carbon Nanofibers

Category Carbon
Manufacturer Nanostructured & Amorphous Materials Inc
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF NanoAmor 95%; OD: 200-500 nm Carbon Nanofibers.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
ApplicationsCatalyst support materialsElectronic devicesFiber/polymer nanocomposites for enhanced electrical conductivityFiber/polymer nanocomposites for enhanced strengthFuel-cell electrodesGas storage (nanoscale gas cylinders)High-power electrochemical capacitorsHigh surface-area electrodesLithium-ion batteriesShielding of electromagnetic radiationInformation provided by NanoAmor Inc.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
True Density
Apparent Bulk Density 0.150 - 0.250 g/cc
0.00542 - 0.00903 lb/in³
Particle Size 0.0010 - 0.010 µm
0.0010 - 0.010 µm
core diameter
0.20 - 0.50 µm
0.20 - 0.50 µm
outside diameter
Specific Surface Area 25 m²/g
25 m²/g
Descriptive Properties Value Comments
Color black
Length (um) 10-40
Purity (vol% carbon nanotubes), min 95