Polymer Property : Apparent Bulk Density = 0.0105 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Apparent Bulk Density 0.290 g/cc
0.0105 lb/in³
NanoAmor 94%, OD/WT/L: 20-50/1-2 nm/0.5-2 um Multi-Walled Carbon Nanotubes
ApplicationsAdditives in polymersCatalystsElectron field emitters for cathode ray lighting elements, flat panel display, gas-discharge tubes in telecom networksElectromagnetic-wave absorption and sh..
Apparent Bulk Density 0.290 - 0.300 g/cc
0.0105 - 0.0108 lb/in³
Average value: 0.298 g/cc Grade Count:8
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Long Glass Fiber Filled". Each property range of values report..
Apparent Bulk Density 0.290 g/cc
0.0105 lb/in³
Sumitomo Bakelite North America 52-20-30 Short-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Information provided by Sumitomo Bak North Americ..
Apparent Bulk Density 0.290 g/cc
0.0105 lb/in³
Cosmic Plastics K61 Long Glass Fiber Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Apparent Bulk Density 0.290 g/cc
0.0105 lb/in³
Cosmic Plastics D69 Long Glass Fiber Filled Ortho Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Apparent Bulk Density 0.290 g/cc
0.0105 lb/in³
Sumitomo Bakelite North America FS-80-P-1 Long-Glass Reinforced Diallyl Phthalate
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GI..