Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Sumitomo Bakelite North America FS-80-P-1 Long-Glass Reinforced Diallyl Phthalate

Category Polymer , Thermoset , Diallyl Phthalate (DAP) , Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled , Filled/Reinforced Thermoset
Manufacturer Sumitomo Bakelite North America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Sumitomo Bakelite North America FS-80-P-1 Long-Glass Reinforced Diallyl Phthalate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Isophthalate DAP Resin Isomer. Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GII-30FInformation provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Density 1.73 g/cc
0.0625 lb/in³
ASTM D792
Apparent Bulk Density 0.290 g/cc
0.0105 lb/in³
Water Absorption 0.30 %
0.30 %
48 hours, 50°C. ASTM D570
Linear Mold Shrinkage 0.0015 - 0.0035 cm/cm
0.0015 - 0.0035 in/in
Compression Molding. ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 88.0 MPa
12800 psi
ASTM D638
Flexural Yield Strength 143 MPa
20700 psi
ASTM D790
Flexural Modulus 13.8 GPa
2000 ksi
ASTM D790
Izod Impact, Notched 3.50 J/cm
6.56 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity 0.335 W/m-K
2.32 BTU-in/hr-ft²-°F
ASTM F433
Maximum Service Temperature, Air 130 °C
266 °F
UL 746B
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
as molded; ASTM D648A
Oxygen Index 41 %
41 %
ASTM D2863
Electrical Properties Metric English Comments
Dielectric Constant 3.3

@Frequency 1000 Hz
3.3

@Frequency 1000 Hz
Wet
Dielectric Strength 15.1 kV/mm
384 kV/in
Wet, step-by-step. ASTM D149
17.1 kV/mm
434 kV/in
Wet, short term. ASTM D149
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
Wet; ASTM D150
Arc Resistance 180 sec
180 sec
ASTM D495
Comparative Tracking Index >= 600 V
>= 600 V
ASTM D3638 (IEC 112)
Processing Properties Metric English Comments
Processing Temperature 160 - 180 °C
320 - 356 °F
Mold temperature