Physical Properties | Metric | English | Comments |
---|---|---|---|
Apparent Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | ASTM D1895 (B) |
ExxonMobil Escorene® UL-7505 EVA Copolymer, Adhesive and Sealant Grade
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A 19.2% vinyl acetate copolymerApplications: Hot melt adhesives; Wax blends; Industrial sealants. |
|||
Apparent Bulk Density | 0.540 - 0.780 g/cc | 0.0195 - 0.0282 lb/in³ | Average value: 0.618 g/cc Grade Count:5 |
Overview of materials for PVC, Transparent This property data is a summary of similar materials in the MatWeb database for the category "PVC, Transparent". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Apparent Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | ASTM D1895 |
Solvay Specialty Polymers Catalyst CT/5-LR UV Polyolefin Catalyst CT/5-LR UV is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan®, Polidiemme® and Co.. |
|||
Apparent Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | ISO 60 |
SolVin 264PC Polyvinyl Chloride General Purpose - Plasticized Made by suspension polymerization.
APPLICATIONS
Extrusion :
- plasticized, semi-rigid, and rigid profiles
- plasticized and rigid pipes
- blowing of plasticized and rigid films
- rigid "pressure" p.. |
|||
Apparent Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | ASTM D1895 |
Solvay Specialty Polymers Catalyst CT/5 UV Polyolefin Catalyst CT/5 is a polyolefin based masterbatch to be used with cable silane crosslinkable compounds in the amount suggested for each material. Developed for Polidan®, Polidiemme® and CogegumÂ.. |
|||
Apparent Bulk Density | 0.540 g/cc | 0.0195 lb/in³ | |
Arkema Group Lacovyl® GB 1350 PVC LACOVYL GB 1350 is a vinyl chloride homopolymer produced by mass polymerization process.CHARACTERISTICS Viscosity index (ISO 1628-2):125 ml/g,(K value:70). Apparent density (ISO 60 ):0.55 g/ml. hig.. |