Apparent Bulk Density 0.370 g/cc
0.0134 lb/in³
Geon® STP 1169; Internal Method
PolyOne Geon™ Specialty Suspension CG E 44 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® CG E44 is a homopolymer specialty suspension resin intended for use in lowering the gloss of extruded or plastisol parts. This resin provides low surface gloss and texturing effects for flexi..
Apparent Bulk Density 0.370 g/cc
0.0134 lb/in³
ASTM D4894
3M Dyneon™ 1750 PTFE Powder  (discontinued **)
Type II PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r..
Apparent Bulk Density 0.370 g/cc
0.0134 lb/in³
Lucobit Lucocell® PE3700 Cellulose Asphalt Additive
Lucocell® PE3700 granules – cellulose additives for SMA –Stone Mastic Asphalt or Split Mastic Asphalt, which is used as finish for all road types. Due to their 3D structure, cellulose f..
Apparent Bulk Density 0.370 g/cc
0.0134 lb/in³
NOVA Chemicals Novapol® TR-0338-UG MDPE Rotational Molding Resin  (discontinued **)
Molded Plaque Properties. Features: Hexene Copolymer, excellent impact strength, excellent ESCR.Applications: large parts, agricultural storage tanks.Data provided by the manufacturer.
Apparent Bulk Density 0.370 g/cc
0.0134 lb/in³
ASTM D4894
Solvay Specialty Polymers Algoflon® F6 PTFE (Polytetrafluoroethylene)  (discontinued **)