PolyOne Geon™ Specialty Suspension CG E 44 Polyvinyl Chloride Homopolymer (PVC Homopolymer)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Specialty Suspension CG E 44 Polyvinyl Chloride Homopolymer (PVC Homopolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Geon® CG E44 is a homopolymer specialty suspension resin intended for use in lowering the gloss of extruded or plastisol parts. This resin provides low surface gloss and texturing effects for flexible vinyl products, allowing the production of broad range of surface effects without the need for secondary operation process which helps to reduce manufacturing cost. The ability to increase surface roughness provides a reduced surface blocking and allows the ease of handling in stacked or bundled parts.Note: The value set forth represent 'typical' values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Packaging: This resin is shipped in multi-wall paper bags, netweight 50lbs, 2,500lbs per pallet. Information shown on the package includes commercial identification number, lot, and weight. STP 488 (formulation): 100phr Geon® CG E44, 55phr TOTM, and 18phr FillerInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
ASTM D792
Volatiles 0.060 %
0.060 %
Geon® STP 793; Internal Method
Apparent Bulk Density 0.370 g/cc
0.0134 lb/in³
Geon® STP 1169; Internal Method
Porosity 0.57 %
0.57 %
cm³/g; Geon® STP 1094; Internal Method
Particle Size <= 105 µm
<= 105 µm
16%; Geon® DFT 1466; Internal Method
150 µm
150 µm
Average Particle SizeGeon® DFT 1466; Internal Method
>= 250 µm
>= 250 µm
4%; Geon® DFT 1466; Internal Method
Descriptive Properties Value Comments
Contamination 0
Internal Method; Magnetic ParticlesGeon® STP 1217 Unit: #/100in2
1
Internal Method; Dark ParticlesGeon® STP 1217 Unit: #/100in2
5
Internal Method; Light Colored ParticlesGeon® STP 1217 Unit: #/100in2
Features Low Gloss
Non-Smooth Surface Finish
Flow Time 34 sec
Internal Method; Conditioned Funnel Flow TimeGeon® STP 1169
Forms Powder
White Powder
Generic Material PVC Homopolymer
Generic Name Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Polymerization Process Suspension
Powder Mix Time 2.8 min
Internal Method; Geon® STP 488 (with provided formula)
Processing Method Dip Coating
Extrusion
Injection Molding
Rotational Molding
Slush Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Residual Vinyl Chloride Monomer < 1 ppm
Internal Method; Geon® STP 1005
Uses Insulation
Wire & Cable Applications
Users viewing this material also viewed the following: