Physical Properties Metric English Comments
Apparent Bulk Density 1.00 - 1.30 g/cc
0.0361 - 0.0470 lb/in³
ISO 60
Raschig Group EN 5004 Epoxy Molding Compound
Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo..
Apparent Bulk Density 1.00 - 1.30 g/cc
0.0361 - 0.0470 lb/in³
ISO 60
Raschig Group EN 5007 Epoxy Molding Compound
Mica reinforced molding compound. Low mold shrinkage and post-shrinkage, very good electrical values, outstanding heat resistance, very goo pourablity. This product meets the allowed upper limits fo..
Apparent Bulk Density 1.00 - 1.15 g/cc
0.0361 - 0.0415 lb/in³
ISO 60
Raschig Group 3572 Epoxy
Glass-fiber reinforced epoxy molding compound. Good mechanical strength and electrical strength, enhanced elasticity for ensuring good sealing under extreme heat and/or humidity, good chemical resis..
Apparent Bulk Density 1.00 g/cc
0.0361 lb/in³
Tap density
Momentive Performance Materials HCJ-48 Boron Nitride (BN) Powder
Grade HCJ-48 is a coarse (-20 mesh), hexagonal Boron Nitride (BN) powder with a mean particle size of 200-250µ. It exhibits the unique properties of BN in a form readily used in the production o..
Apparent Bulk Density 1.00 - 1.20 g/cc
0.0361 - 0.0434 lb/in³
Johnson Matthey Yara 58-Y1 N2O Abatement Catalyst
Odorless solid pellets, 9 x 9 mm. During the manufacture of Nitric Acid, significant quantities of pollutants are released into the atmosphere. One of the principal pollutants is the greenhouse gas..
Apparent Bulk Density 1.00 g/cc
0.0361 lb/in³
ASTM D1895
Sumitomo Bakelite Durez® 29502 B Phenolic, Compression Grade
Durez 29502 B brown phenolic is a two stage, glass and mineral filled, special purpose molding material with improved mechanical and heat resistant properties. It is formulated for close tolerance ..
Apparent Bulk Density 1.00 g/cc
0.0361 lb/in³
Arkema Group VOLTALEF® 302 PCTFE
VOLTALEF® 302 is a chlorotrifluoroethylene dense powder. Used in particular for compression molding, non-flammable. Information provided by Arkema Group
Apparent Bulk Density 1.00 g/cc
0.0361 lb/in³
Tap density
Carborundum CarboTherm™ CTH40 Boron Nitride Powder
Boron Nitride powders have high thermal conductivity, low dielectric loss, and low thermal expansion. They are non-abrading to electronic components, lubricious, non-toxic, and retain their dielect..