Physical Properties Metric English Comments
Saybolt Viscosity at 100°F 795 SUS
795 SUS
Base Oil Property
ConocoPhillips Tacna® Rx NLGI No. 1
Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motor..
Saybolt Viscosity at 100°F 795 SUS
795 SUS
Base Oil Property
ConocoPhillips Tacna® Rx NLGI No. 2
Description: Conoco Tacna Rx is a multipurpose, lithium-complex, polymer-enhanced grease designed for a wide range of applications, including passenger cars, agricultural equipment, race cars, motor..