Physical Properties Metric English Comments
Saybolt Viscosity at 210°F 75 SUS
75 SUS
Base Oil Property
ConocoPhillips Syncon® HP Synthetic Grease NLGI No. 1
Description: Conoco Syncon HP Synthetic Grease is a high-quality, synthetic polyalphaolefin (PAO) lithium grease developed to provide exceptional protection and corrosion resistance for bearings and..
Saybolt Viscosity at 210°F 75 SUS
75 SUS
ChevronTexaco 150 PMO Premium
Texaco PMO Premium oils deliver value through:Minimized unscheduled downtime — High oxidation stability provides excellent resistance to deposit formation. The detergent/dispersant additive system ..
Saybolt Viscosity at 210°F 75 SUS
75 SUS
ChevronTexaco MP Drive Train Fluid
FeaturesChevron Drive Train Fluid - MP is a multipurpose lubricant designed for use in transmissions, wet brakes, and hydraulic systems requiring a fluid meeting Caterpillar TO-4 or TO-4M requiremen..
Saybolt Viscosity at 210°F 75 SUS
75 SUS
ASTM D-2161
ConocoPhillips ANDEROL® AA-40 White Mineral Food Grade Oil, ISO Grade 150, SAE Grade 40
Description: ANDEROL PQ AA Series Oils are white mineral oil based products that meet the former H-1 approval requirements of the USDA where incidental food contact can occur. PQ AA Series Oils are ..
Saybolt Viscosity at 210°F 75 SUS
75 SUS
ChevronTexaco ISO 150 Industrial Oil EP
FeaturesChevron Industrial Oils EP are multipurpose oils for industrial service.Chevron Industrial Oils EP are designed to help minimize wear in all types of plant lubrication and also provide long ..