Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.0800 - 150 g/10 min | 0.0800 - 150 g/10 min | Average value: 11.3 g/10 min Grade Count:448 |
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and.. |
|||
Melt Flow | 0.0800 - 80.0 g/10 min | 0.0800 - 80.0 g/10 min | Average value: 14.7 g/10 min Grade Count:399 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Molded". Each property range of values reported is minimum and ma.. |