Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.92 g/10 min @Load 2.16 kg, Temperature 230 °C |
0.92 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Topas Advanced Polymers TOPAS® 6013F-04 Cyclic Olefin Copolymer (COC) TOPAS® 6013F-04 is a high temperature, general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and p.. |