Physical Properties Metric English Comments
Melt Flow 0.92 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.92 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Topas Advanced Polymers TOPAS® 6013F-04 Cyclic Olefin Copolymer (COC)
TOPAS® 6013F-04 is a high temperature, general purpose film extrusion grade. It is a high clarity amorphous resin with high stiffness, moisture barrier, chemical resistance, thermoformability and p..