Physical Properties Metric English Comments
Melt Flow 0.96 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.96 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 58G (High Gloss) HDPE Blow Molding Resin  (discontinued **)
Features: Outstanding gloss, pearlescent finish when colored, good processability.Applications: Small part blow molding, injection blow molding, low-moderate ESCR uses.Data provided by the manufactu..
Melt Flow 0.96 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.96 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
NOVA Chemicals Sclair® 14L1 Octene LMDPE Film Resin  (discontinued **)
Low gel, Good clarity, Excellent sealing characteristicsApplications: Lamination, Co-extrusionAdditives: Process stabilizer, polymer process aidFilm properties are typical of blown film extruded at ..
Melt Flow 0.96 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.96 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Arkema Group Evatane® 1005 VN 5 Ethylene Vinyl Acetate
EVA copolymer made by high pressure tubular process. Applications Grade for films with high transparency and high mechanical properties. Examples: coextrusion, stretch film, paper-stationary, fancy ..