Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 13.9 g/10 min | 13.9 g/10 min | Condition S; ASTM D 1238 |
CPT C-Flex® R70-089 Opaque Biocompatible TPE C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current.. |
|||
Melt Flow | 13.9 g/10 min | 13.9 g/10 min | 220C/10,000 g; ASTM D1238 |
Albis Plastics ASA 02A MR20 , 20% Mineral Filled
(discontinued **) Acrylonitrile/Styrene/AcrylateCharacteristics: Excellent UV, Good Rigidity, Good Dimensional StabilityApplications: Sunglasses, Boat Shells, Roofs for Campers & RVsProcessing: Injection Molding (Mel.. |