Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 14.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
14.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom PLASTAMID® 6 BT N 29 B/IM PA6 Basic type PA 6 for injection molding, for general use. Use: automotive, engineering, electrical and consumer-goods industry - electrical tools, fasteners, clamps, hobby tools. Delivered in the natu.. |
|||
Melt Flow | 14.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
14.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Asia Pacific) Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 920 PC Opaque colors, low viscosity, superior flame retardance. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 920 PC (Asia Pacific) Opaque colors, low viscosity, superior flame retardance. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 920A PC Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 923 PC Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 923 PC (Asia Pacific) Opaque colors, low viscosity, superior flame retardance. Decreased smoke and lowered toxic gas emission. UV-stabilized. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 923A PC Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 923A PC (Asia Pacific) Low viscosity, flame retardant with exceptional surface. Clear, tints and opaque colors. UV-stabilized. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 923ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. UV-stabilized. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Europe-Africa-Middle East) This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® DMX9455 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX9455 is a standard flow, flame retardant, V0/1.5mm, opaque polycarbonate copolymer resin with improved scratch resistance. |
|||
Melt Flow | 14.5 g/10 min @Load 2.16 kg, Temperature 260 °C |
14.5 g/10 min @Load 4.76 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 920A PC (Asia Pacific) Low viscosity injection moldable, flame retardant PC. Exceptional surface appearance. Clear, tints and opaque colors. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 920ASR PC More robust design of standard 900 series flame retardant grade. Internal mold release. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® DMX1435 PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX1435 is a UV stabilized standard flow polycarbonate copolymer resin with improved scratch resistance. |
|||
Melt Flow | 14.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
14.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® DMX9455A PC Copolymer (Asia Pacific) This product will be phased out per January 2015 -- Lexan* DMX9455A is a standard flow, flame retardant, transparent polycarbonate copolymer resin with improved scratch resistance. |
|||
Melt Flow | 14.5 g/10 min @Load 5.00 kg, Temperature 230 °C |
14.5 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 1-5140 BLH 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-5140 BLH is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-5140 BLH is recommended especially for producing products, where high stiffn.. |
|||
Melt Flow | 14.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
14.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D 1238 |
Styrolution PS 5801 HIPS Exceptional processabilityHigh toughnessUSP Class VI certifiedUl Classification 94 HBInformation provided by Styrolution |
|||
Melt Flow | 14.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
14.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Dow TF0807 TPO Dow Fascia TPO for Painted ApplicationsInformation provided by Dow |
|||
Melt Flow | 14.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
14.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
DIN 5375/ISO 1133 |
Ineos Nova S-3201 Medium Impact Compact Polystyrene
(discontinued **) Extremely easy flowing medium impact polystyrene, designed for extreme short cycle times for injection molding of household, packaging and toys. The material is provided with external lubricant to .. |
|||
Melt Flow | 14.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
14.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H14A-00 Polypropylene Homopolymer Suggested fabrication methods: Injection molding and extrusion applications.Features: AntistaticTypical applications: Packaging, Closures, Consumer productsComplies with FDA specification, Title 21,.. |