Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.900 - 16.9 g/10 min | 0.900 - 16.9 g/10 min | Average value: 7.80 g/10 min Grade Count:3 |
Overview of materials for Polycarbonate, Conductive This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Conductive". Each property range of values reported is minimum and maximum values of appr.. |
|||
Melt Flow | 13 - 16.9 g/10 min | 13 - 16.9 g/10 min | |
Shuman 502 Black Polypropylene Copolymer Good impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer. |
|||
Melt Flow | 13 - 16.9 g/10 min | 13 - 16.9 g/10 min | |
Shuman 502C Black Polypropylene Copolymer Excellent impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer. |
|||
Melt Flow | 13 - 16.9 g/10 min | 13 - 16.9 g/10 min | |
Shuman 510 Black Polypropylene Homopolymer Excellent chemical resistance, excellent processabilityData provided by the manufacturer. |