Material Notes:
Good impact strength, excellent chemical resistance, excellent processability, good wear and abrasion resistance, good resistance to fatigue from flexing.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D792
Melt Flow 5.0 - 8.9 g/10 min
5.0 - 8.9 g/10 min
ASTM D1238
9.0 - 12.9 g/10 min
9.0 - 12.9 g/10 min
13 - 16.9 g/10 min
13 - 16.9 g/10 min
17.0 - 22.0 g/10 min
17.0 - 22.0 g/10 min
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Izod Impact, Notched 0.850 J/cm
1.59 ft-lb/in
MIN; Notched; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 47.0 °C
117 °F
ASTM D648
Vicat Softening Point 149 °C
300 °F
ASTM D1525
Processing Properties Metric English Comments
Processing Temperature 188 - 216 °C
370 - 421 °F