Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.0 - 17.5 g/10 min @Load 3.80 kg, Temperature 232 °C |
4.0 - 17.5 g/10 min @Load 8.38 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Melt Flow | 4.0 - 17.5 g/10 min @Load 3.80 kg, Temperature 232 °C |
4.0 - 17.5 g/10 min @Load 8.38 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 2950-05 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Very flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Melt Flow | 4.0 - 17.5 g/10 min @Load 3.80 kg, Temperature 232 °C |
4.0 - 17.5 g/10 min @Load 8.38 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |