Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 18.5 g/10 min @Load 2.16 kg, Temperature 330 °C |
18.5 g/10 min @Load 4.76 lb, Temperature 626 °F |
cm³/10 min. |
Covestro Apec® DP 1-9359/7 Polycarbonate
(discontinued **) Key Features:Release agentUnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer M.. |
|||
Melt Flow | 18.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
18.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX942 PPE+PS+PA66 Noryl GTX* GTX942 Resin is a blend of Polyphenylene Ether(PPE) + Polyamide(PA) resin that is designed to have high melt flow for large part/thinwall injection molding. The material is designed to h.. |
|||
Melt Flow | 18.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
18.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® FR6901 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Flame retardant• Hig.. |