Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 19.8 g/10 min @Load 1.20 kg, Temperature 300 °C |
19.8 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Lehmann & Voss LUVOCOM® 50/TF/15/BK7284 Polycarbonate, with PTFE, easy flowing Applications: Data processing machinery, precision engineering, film and photo industry, sporting and leisure goods, medical enineering.Improved friction and wear behaviour. Emergency running proper.. |
|||
Melt Flow | 19.8 g/10 min @Load 5.00 kg, Temperature 300 °C |
19.8 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL PX2938 PPE (Asia Pacific) PPE+PS GF20% High Heat FR V-0 |