SABIC Innovative Plastics NORYL PX2938 PPE (Asia Pacific)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name Noryl
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics NORYL PX2938 PPE (Asia Pacific).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PPE+PS GF20% High Heat FR V-0
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Water Absorption 0.060 %

@Time 86400 sec
0.060 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm

@Thickness 3.20 mm
0.0020 - 0.0040 in/in

@Thickness 0.126 in
SABIC Method
Melt Flow 19.8 g/10 min

@Load 5.00 kg,
Temperature 300 °C
19.8 g/10 min

@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 127
127
ASTM D785
Tensile Strength, Yield 107 MPa
15500 psi
SABIC - Japan Method
Elongation at Break 8.0 %
8.0 %
SABIC - Japan Method
Flexural Strength 143 MPa
20700 psi
ASTM D790
Flexural Modulus 5.64 GPa
818 ksi
ASTM D790
Izod Impact, Notched 0.870 J/cm
1.63 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear 27.0 - 44.0 µm/m-°C

@Temperature -30.0 - 30.0 °C
15.0 - 24.4 µin/in-°F

@Temperature -22.0 - 86.0 °F
TMA
Deflection Temperature at 1.8 MPa (264 psi) 143 °C

@Thickness 6.40 mm
289 °F

@Thickness 0.252 in
unannealed; ASTM D648