Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.00 - 198 g/10 min | 1.00 - 198 g/10 min | Average value: 31.9 g/10 min Grade Count:71 |
Overview of materials for Nylon 66, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. .. |
|||
Melt Flow | 1.00 - 198 g/10 min | 1.00 - 198 g/10 min | Average value: 59.2 g/10 min Grade Count:59 |