Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.30 g/10 min @Load 2.16 kg, Temperature 230 °C |
2.30 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4465A Thermoplastic Elastomer Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;.. |
|||
Melt Flow | 2.30 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.30 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® LD 768.MJ Molding, extrusion and compounding resin Escorene Ultra LD 768.MJ is a high viscosity, 26.2% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be .. |
|||
Melt Flow | 2.30 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.30 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® UL 7765 Adhesive Application Resin Escorene Ultra UL 7765 is a high viscosity, 26.2% vinyl acetate copolymer that has very good flexibility and low temperature toughness. It has good compatibility with both hydrocarbon and natural t.. |