Polymer Property : Melt Flow = 2.30 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 2.30 g/10 min

@Load 2.16 kg,
Temperature 230 °C
2.30 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Teknor Apex Telcar® OBC 4465A Thermoplastic Elastomer
Uses: Blow Molding Applications; General Purpose; Soft Touch Applications Forms: Pellets Processing Method: Blow Molding; Profile Extrusion; Sheet Extrusion; Thermoforming; Wire and Cable Extrusion;..
Melt Flow 2.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escorene® LD 768.MJ Molding, extrusion and compounding resin
Escorene Ultra LD 768.MJ is a high viscosity, 26.2% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be ..
Melt Flow 2.30 g/10 min

@Load 2.16 kg,
Temperature 190 °C
2.30 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
ExxonMobil Escorene® UL 7765 Adhesive Application Resin
Escorene Ultra UL 7765 is a high viscosity, 26.2% vinyl acetate copolymer that has very good flexibility and low temperature toughness. It has good compatibility with both hydrocarbon and natural t..