Physical Properties Metric English Comments
Melt Flow 200 g/10 min

@Load 2.16 kg,
Temperature 190 °C
200 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polimeri Europa Riblene® MY 00 Low Density Polyethylene - Injection Molding
Riblene MY 00 is a very high flowability low density polyethylene resin (LDPE).Main Applications: Riblene MY 00 is suitable for hot melts.Information provided by Polimeri Europa.
Melt Flow 200 g/10 min

@Load 2.16 kg,
Temperature 190 °C
200 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Eastman 812A Polyethylene  (discontinued **)
Polyethylene 812A is a natural low density material with a 200 melt index. This high-flow formulation is used for specialty injection molding applications in the medical market.Unless otherwise not..
Melt Flow 200 g/10 min

@Load 2.16 kg,
Temperature 190 °C
200 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Eastman 812P Polyethylene  (discontinued **)
Polyethylene 812A is a natural low density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a carpet backing to bind fibers to the carpet...
Melt Flow 200 g/10 min
200 g/10 min
ISO 1133-1981E
LyondellBasell Montell 0800 Polybutene
Key Features: highly isotactic, semi-crystalline homopolymer, good creep resistance, good environmental crack resistance, miscible with polypropylenes, FDA acceptableApplications: concrete carrierMe..
Melt Flow 200 g/10 min

@Load 2.16 kg,
Temperature 190 °C
200 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Polyram Bondyram® 1010 Maleic Anhydride Modified Polypropylene
Information provided by Polyram.
Melt Flow 200 g/10 min

@Load 2.16 kg,
Temperature 190 °C
200 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Westlake EC812AA Low Density Polyethylene
WESTLAKE low-density polyethylene EC812 is a natural low-density material with a 200 melt index. Its high melt index exhibits excellent wettability. This makes it ideal as a backing to carpet to bin..
Melt Flow 200 g/10 min

@Load 2.16 kg,
Temperature 190 °C
200 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Westlake EM812AA Low Density Polyethylene
WESTLAKE low-density polyethylene EM812 is a low-density formulation used for injection molding. It is an outstanding material for molding lids and other container closures because it processes easi..
Melt Flow 200 g/10 min

@Load 2.16 kg,
Temperature 190 °C
200 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Celanese 192 LDPE polymer for adhesives, automotive and compounds