Polymer Property : Melt Flow = 23.8 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 16.5 - 23.8 g/10 min
16.5 - 23.8 g/10 min
Average value: 20.5 g/10 min Grade Count:5
Overview of materials for Polybutylene Terephthalate (PBT), PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and ma..