  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), PTFE Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.33 - 1.65 g/cc
0.0480 - 0.0596 lb/in³
Average value: 1.42 g/cc Grade Count:31
Filler Content 10.0 - 20.0 %
10.0 - 20.0 %
Average value: 14.1 % Grade Count:8
Water Absorption 0.0500 - 0.150 %
0.0500 - 0.150 %
Average value: 0.0867 % Grade Count:15
Additive Loading 5.00 - 10.0 %
5.00 - 10.0 %
Average value: 6.67 % Grade Count:3
Linear Mold Shrinkage 0.000700 - 0.0250 cm/cm
0.000700 - 0.0250 in/in
Average value: 0.0183 cm/cm Grade Count:29
Melt Flow 16.5 - 23.8 g/10 min
16.5 - 23.8 g/10 min
Average value: 20.5 g/10 min Grade Count:5
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 33.0 - 100 MPa
4790 - 14500 psi
Average value: 47.4 MPa Grade Count:29
Tensile Strength, Yield 43.0 - 53.1 MPa
6240 - 7700 psi
Average value: 47.9 MPa Grade Count:3
Elongation at Break 3.00 - 12.0 %
3.00 - 12.0 %
Average value: 8.85 % Grade Count:19
Elongation at Yield 2.80 - 12.0 %
2.80 - 12.0 %
Average value: 5.13 % Grade Count:10
Modulus of Elasticity 2.00 - 6.00 GPa
290 - 870 ksi
Average value: 2.67 GPa Grade Count:26
Flexural Yield Strength 50.0 - 100 MPa
7250 - 14500 psi
Average value: 73.8 MPa Grade Count:25
Flexural Modulus 1.70 - 4.00 GPa
247 - 580 ksi
Average value: 2.37 GPa Grade Count:28
Izod Impact, Notched 0.320 - 0.694 J/cm
0.600 - 1.30 ft-lb/in
Average value: 0.495 J/cm Grade Count:18
Izod Impact, Unnotched 3.47 - 8.54 J/cm
6.50 - 16.0 ft-lb/in
Average value: 5.84 J/cm Grade Count:14
Izod Impact, Notched (ISO) 3.00 - 7.00 kJ/m²
1.43 - 3.33 ft-lb/in²
Average value: 4.65 kJ/m² Grade Count:4
6.00 - 6.00 kJ/m²

@Temperature -30.0 - -30.0 °C
2.86 - 2.86 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 6.00 kJ/m² Grade Count:1
Charpy Impact Unnotched 1.90 - 3.50 J/cm²
9.04 - 16.7 ft-lb/in²
Average value: 2.54 J/cm² Grade Count:9
Charpy Impact, Notched 0.150 - 0.500 J/cm²
0.714 - 2.38 ft-lb/in²
Average value: 0.317 J/cm² Grade Count:3
Coefficient of Friction 0.120 - 0.390
0.120 - 0.390
Average value: 0.188 Grade Count:8
Coefficient of Friction, Static 0.0800 - 0.210
0.0800 - 0.210
Average value: 0.129 Grade Count:8
Thermal Properties Metric English Comments
CTE, linear 32.4 - 109 µm/m-°C
18.0 - 60.6 µin/in-°F
Average value: 76.5 µm/m-°C Grade Count:3
Maximum Service Temperature, Air 130 - 150 °C
266 - 302 °F
Average value: 140 °C Grade Count:8
Deflection Temperature at 0.46 MPa (66 psi) 143 - 215 °C
290 - 419 °F
Average value: 166 °C Grade Count:4
Deflection Temperature at 1.8 MPa (264 psi) 54.4 - 190 °C
130 - 374 °F
Average value: 68.7 °C Grade Count:21
Vicat Softening Point 165 - 210 °C
329 - 410 °F
Average value: 183 °C Grade Count:5
Flammability, UL94 HB - V-0
HB - V-0
Grade Count:18
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+14 - 3.00e+16 ohm-cm
1.00e+14 - 3.00e+16 ohm-cm
Average value: 1.00e+16 ohm-cm Grade Count:10
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
Average value: 1.00e+14 ohm Grade Count:3
Insulation Resistance 1.00e+12 ohm
1.00e+12 ohm
Average value: 1.00e+12 ohm Grade Count:8
Processing Properties Metric English Comments
Processing Temperature 232 - 270 °C
450 - 518 °F
Average value: 250 °C Grade Count:11
Nozzle Temperature 250 - 265 °C
482 - 509 °F
Average value: 258 °C Grade Count:8
Melt Temperature 230 - 280 °C
446 - 536 °F
Average value: 257 °C Grade Count:26
Mold Temperature 49.0 - 120 °C
120 - 248 °F
Average value: 88.1 °C Grade Count:29
Drying Temperature 80.0 - 121 °C
176 - 250 °F
Average value: 108 °C Grade Count:27
Moisture Content 0.0300 - 0.150 %
0.0300 - 0.150 %
Average value: 0.0447 % Grade Count:15
Dew Point -28.9 °C
-20.0 °F
Average value: -28.9 °C Grade Count:12
Injection Pressure 4.96 - 103 MPa
720 - 15000 psi
Average value: 75.9 MPa Grade Count:14
Copyright © lookpolymers.com All Rights Reserved