Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 29.6 g/10 min @Load 10.0 kg, Temperature 380 °C |
29.6 g/10 min @Load 22.0 lb, Temperature 716 °F |
|
Lehmann & Voss LUVOCOM® 1105-7909/GY 2 PEEK, with carbon fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts.Dynamic stressed parts at high movement velocity.Chemical and hydrolys.. |
|||
Melt Flow | 29.6 g/10 min @Load 2.16 kg, Temperature 190 °C |
29.6 g/10 min @Load 4.76 lb, Temperature 374 °F |
|