Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.20 - 56.0 g/10 min | 3.20 - 56.0 g/10 min | Average value: 25.3 g/10 min Grade Count:24 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Melt Flow | 3.20 - 12.9 g/10 min | 3.20 - 12.9 g/10 min | Average value: 6.37 g/10 min Grade Count:7 |
Overview of materials for Nylon 12, 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, 20% Glass Fiber Filled". Specific grades with glass content between 15% and 24% are included. .. |
|||
Melt Flow | 3.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Optema® TC-114 Blown Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elast.. |
|||
Melt Flow | 3.20 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.20 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate Product Description: Optema TC 114 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown and cast film applications. It produces a so.. |