Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.50 - 54.0 g/10 min | 3.50 - 54.0 g/10 min | Average value: 22.6 g/10 min Grade Count:4 |
Overview of materials for PVC, Rigid Grade This property data is a summary of similar materials in the MatWeb database for the category "PVC, Rigid Grade". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Melt Flow | 3.50 g/10 min @Load 21.6 kg, Temperature 190 °C |
3.50 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinvicomp SBC 3707 Polyvinyl Chloride, Rigid Notes: RoHS Compliant Availability: Asia Pacific Features: Food Contact Acceptable; Medium Impact Resistance Uses: Bottles; Containers Forms: Pellets Processing Method: Blow MoldingInformation Provi.. |
|||
Melt Flow | 3.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 4530A Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 3.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL EF-6109 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 3.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL EF-6162 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 3.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-4001C Thermoplastic Elastomer Notes: UV Stabilized Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstrip.. |
|||
Melt Flow | 3.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Uniprene® UN-2678C Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Flow | 3.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ExxonMobil Method |
ExxonMobil Escorene® LD 713.93 Blown Film Resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhibits very high impact strength, high clarity, and excellent heat sealability.Availability: Lat.. |
|||
Melt Flow | 3.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ExxonMobil Method |
ExxonMobil Escorene® LD 713.93 Cast Film Resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer film resin. Film made from LD 713.93 exhbits very high impact strength, hihg clarity, and excellent heat sealabilityAvailability: Latin.. |
|||
Melt Flow | 3.50 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.50 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® LD 713.93 Molding, extrusion and compounding resin Escorene Ultra LD 713.93 is a 14.4 wt% vinyl acetate copolymer with very good toughness, high clarity and excellent processability. It is suitable for use in making molded articles, extruded profile.. |
|||
Melt Flow | 3.50 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.50 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron SE45I Extrusion ABS Very High Impact, Low Flow, High Rigidity and Sheet/Pipe/Profile applicationInformation provided by Bhansali |
|||
Melt Flow | 3.50 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.50 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Bhansali Engineering Abstron SE45I Extrusion ABS Very High Impact, Low Flow, High Rigidity and Sheet/Pipe/Profile applicationInformation provided by Bhansali |