Polymer Property : Melt Flow = 34.75 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Melt Flow 34.75 g/10 min

@Load 2.16 kg,
Temperature 240 °C
34.75 g/10 min

@Load 4.76 lb,
Temperature 464 °F
Calculated from 25cm3/10min volume-flow rate; ISO 1133
DSM Arnitel® PL460-S 46 Shore D Copolyester Elastomer, Injection Grade (Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Melt Flow 34.75 g/10 min

@Load 2.16 kg,
Temperature 240 °C
34.75 g/10 min

@Load 4.76 lb,
Temperature 464 °F
Calculated from Volume Flow Rate of 25 cm<sup>3</sup>/10 min; ISO 1133
DSM Arnitel® PL460-S 46 Shore D, Injection Grade, Flame Retardant Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..