Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 34.75 g/10 min @Load 2.16 kg, Temperature 240 °C |
34.75 g/10 min @Load 4.76 lb, Temperature 464 °F |
Calculated from 25cm3/10min volume-flow rate; ISO 1133 |
DSM Arnitel® PL460-S 46 Shore D Copolyester Elastomer, Injection Grade (Asian Grade) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |
|||
Melt Flow | 34.75 g/10 min @Load 2.16 kg, Temperature 240 °C |
34.75 g/10 min @Load 4.76 lb, Temperature 464 °F |
Calculated from Volume Flow Rate of 25 cm<sup>3</sup>/10 min; ISO 1133 |
DSM Arnitel® PL460-S 46 Shore D, Injection Grade, Flame Retardant Copolyester Elastomer (North America) Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn.. |